Polycyclohexylenedimethylene terephthalate

Polycyclohexylenedimethylene terephthalate (PCT) is a thermoplastic polyester formed from the polycondensation of terephthalic acid and cyclohexanedimethanol.[1] Its chemical structure is similar to that of polyethylene terephthalate (PET), with which it shares properties like dimensional stability and chemical resistance. PCT is also particularly resistant to high temperatures and hydrolysis. The melting point is 545 °F (285 °C). Common brand names are Thermx (Ticona), Eastar (Eastman) and SkyPURA (SK Chemicals).

Polycyclohexylenedimethylene terephthalate
Identifiers
ChemSpider
  • none
Properties
Melting point 285 °C (545 °F; 558 K)
Except where otherwise noted, data are given for materials in their standard state (at 25 °C [77 °F], 100 kPa).
Infobox references

Application

Polycyclohexylenedimethylene terephthalate has good dimensional stability at excess temperatures (short-term up to 493 °F (256 °C)) making this material suitable for injection molding of thin-walled parts. PCT is used for electronics components like plug connectors. PCT is also processed into filaments, fibers, and fabrics that are used in industry as filters. The color stability and lower density are of advantage in other applications, especially in the LED reflector application.

References

  1. Horst Köpnick, Manfred Schmidt, Wilhelm Brügging, Jörn Rüter, Walter Kaminsky (2002). "Polyesters". Ullmann's Encyclopedia of Industrial Chemistry. Weinheim: Wiley-VCH. doi:10.1002/14356007.a21_227. ISBN 3527306730.CS1 maint: uses authors parameter (link)